Hardish landing broke blade fus just aft of wing at site of previous repair that had just used glue and a bit of bondo from what I could see.

Used large diameter heatshrink+paper towels+perforated release film.
Resin was same weight as Kevlar

Lay up = 924 transfer tape (applied to Kevlar to hold in place on fus)
105 Wests laminating resin stippled on and then excess removed with paper towels.
perforated release film
paper towels
transparent...Continue Reading